Product details
Minimum Order Quantity | 200 Kilogram |
Coefficient of thermal expansion at Degree C | 20-600 Deg C |
Cooling | Furnace |
Hardening Degree C | 840-900 Deg C |
Hardness after quenching HRC | 55-57 HRC |
Hardness HB | Max 240 |
Soft annealing Degree C | 650-710 Deg C |
Thermal Conductivity at Degree C | 20-700 Deg C |
Width | 130 to 1600 mm |
Thickness | 125 to 1000 mm |
Technique | Hot Rolled |
Shape | Rectangular |
Usage/Application | Construction |
Chemical Composition - (Typical Analysis in %)
STANDARDS | 55NiCrMoV7 | DB6 | DIN 2714 | AISI L6 | AFNOR 55NCDVV7 | JIS SKT4 |
C | Si | Mn | P | S | Cr | Ni | Mo | V |
0.50-0.60 | 0.10-0.40 | 0.65-0.95 | <0.015 | <0.004 | 1.0-1.20 | 1.50-1.80 | 0.45-0.55 | 0.07-0.12 |
USA | Europe | Germany | China | Japan | India | R. of Korea | Russia |
AISI / SAE | En | DIN, WNr | GB | JIS | IS | KS | GOST |
A681 L6 | 55NiCrMoV7 | 56NiCrMoV7 | 5CrNiMo | SKT4 | T55Ni7Cr4Mo5V1 | STF4 | 4ChMNFS |