Supported by dedication of our adept professionals, we are engaged in offering excellent quality 2379 Die Steel to our prestigious clients. It is used in tooling applications where high wear resistance is required. This die steel hardens after air cooling to ensure no deformation after heat treatment. It is fabricated with use of cutting edge technology under proper supervision of our experts. Apart from this, 2379 Die Steel is available with us at very affordable prices keeping in mind budget of customers. Also, it is highly efficient product that has excelled in market by virtue of its outstanding durability as well as dimensional stability.
Technical Specification
C | Si | Mn | P | S | Cr | Ni | Mo | V |
1.40-1.60 | 0.10-0.60 | 0.20-0.60 | 0.040max | 0.040 max | 11.00-13.00 | 1.65-2.00 | 0.70-0.100 | 0.80-1.20 |
Coefficient Conductivity at °C | 10-8W/ (m*K) |
20-100 | 10.6 |
20-200 | 11.5 |
20-300 | 11.8 |
20-400 | 12.3 |
Thermal Conductivity at °C | W(m*k) |
20 | 16.7 |
350 | 20.5 |
700 | 24.2 |
Heat Treatment
Soft Annealing °C | 840-870 |
Cooling | Furnace |
Hardness HB | Max. 250 |
Stress-relief Annealing °C | Approx. 66-710 |
Hardening °C | 1000-1050 |
Quenching | Air, oil salt bath 500-550°C |
Hardness after Quenching HRC | 63 |