Product details
Minimum Order Quantity | 200 Kg |
Coefficient of thermal expansionat Degree C | 20-700 Deg C |
Cooling | Furnace |
Hardness after quenching HRC | 55 HRC |
Hardness HB | Max 240 |
Soft annealing Degree C | 760 - 810 Deg C |
Thermal Conductivity Degree C | 20-700 Deg C |
Width | 40 to 700 mm |
Thickness | 20 to 400 mm |
Technique | Hot Rolled |
Shape | Rectangular |
Usage/Application | Construction |
Chemical Composition - (Typical Analysis in %)
STANDARDS | X40CrMoV5 | H13 | DIN 2344 | AISI H13 | AFNOR Z40CDV5 | JIS SKD61 |
C | Si | Mn | P | S | Cr | Mo | V |
0.35-0.45 | 0.90-1.20 | 0.30-0.50 | <0.03 | <0.004 | 4.90-5.40 | 1.20-1.75 | 0.90-1.20 |
VENTURA ALLOY AND STEELS PRIVATE LIMITED
All Rights Reserved.(Terms of Use) Developed and Managed by Infocom Network Private Limited. |