Product details
Cooling | Furnace |
Hardening | 840-870 Deg C |
Hardness | Max. 235 HB |
Hardness After Quenching | 51 HRC |
Material Grade | HCHCR D3 |
Quenching | Polymer or Oil |
Soft Annealing | 710-740 Deg C |
Technique | Hot Rolled |
Shape | Rectangular |
Application | Construction |
CHEMICAL COMPOSITION (Typical Analysis in %
STANDARDS | X210CrW12 | HCHCR-D3 | DIN 2080 | AISI D3 | AFNOR Z210W12-01 | JIS SKD1 |
C | Si | Mn | P | S | Cr |
2.00-2.35 | 0.10-0.60 | 0.20-0.60 | 0.030max | 0.030max | 11.00-13.00 |
PHYSICAL PROPERTIES
Coefficient of Thermal Expansion at °C | 10¯ m / (m*K) |
20-100 | 10.7 |
20-200 | 11.6 |
20-300 | 12.3 |
20-400 | 12.6 |
20-500 | 12.9 |
20-600 | 13.2 |
20-700 | 13.3 |
Thermal Conductivity at °C | W / (m*K) |
20 | 16.6 |
350 | 20.5 |
700 | 24.3 |
VENTURA ALLOY AND STEELS PRIVATE LIMITED